Process for producing a positive electrode for a non-aqueous electrolytic cell
Abstract
Disclosed is a process for producing a positive electrode for a non-aqueous electrolytic cell. Manganese dioxide is heat-treated at a temperature between 250° and 400° C. The heat-treated manganese dioxide is next mixed with a conducting agent and binder. The binder is suspended in water by means of non-ionic surface active agent, and the mixture is heat-treated at a temperature between 180° and 350° C. and then pressured molded into a positive electrode. This production process allows the provision of a positive electrode for a non-aqueous electrolytic cell of excellent discharge characteristics.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 25.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for producing a positive electrode for a non-aqueous electrolytic cell comprising the steps of: (a) heat-treating manganese dioxide; (b) adding the thus heat-treated manganese dioxide with a conducting agent and a binder to be mixed together; (c) heat-treating the resultant mixture; and (d) molding the thus heat-treated mixture to form a positive electrode.
- Claim 2Depends on #1
A process according to claim 1, wherein said binder is suspended in a dispersion medium by means of a dispersing agent.
- Claim 3Depends on #1, #2
A process according to claim 1 or 2, wherein said binder comprises fine powders of a fluorine-containing resin and said fine powders of said fluorine-containing resin are suspended in water or an organic solvent by means of a non-ionic surface active agent.