Patents
US 4,297,149 A#22525138 Most CitedExpiredUnited States (USPTO)Utility

Method of treating SiPOS passivated high voltage semiconductor device

4Forward Citations (#22525138 Global)
0.1/yrCitation Velocity (#46434833 Global)
5.80Citation PageRank (#2599626 Global)
4Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The breakdown voltage of high voltage semiconductor devices passivated with SiPOS deteriorates if the devices are allowed to soak at temperatures in the 400° C. to 525° C. range. The original breakdown voltage is recovered by annealing the devices at a temperature of above about 550° C. prior to metallization and alloying the metal at less than 425° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    In a process of fabricating a semiconductor device having oxygenated polycrystalline silicon passivation layers the improvement comprising: annealing the devices at at least 525° C. prior to metallization; cooling the devices rapidly through the 500° C. to 450° C. temperature range at the end of said annealing; preventing the devices from subsequently being heated to any temperature higher than 425° C.; and preventing the devices from being exposed to any temperature above 400° C. for longer than a total of ten minutes subsequent to the annealing whereby the devices will have near the ma

  2. Claim 2Depends on #1

    The method recited in claim 1 wherein: said annealing step is performed at a temperature of at least 550° C.

  3. Claim 3Depends on #1

    The method recited in claim 1 wherein: said

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗