Method of manufacturing rolled steel products with high elastic limit
Abstract
A rolled steel product is given an elastic limit of 500 to 1200 MPa by selection of a particular steel composition and a particular heat treatment. The steel contains 0.10-0.50% C, 0.90-1.50% Mn, and 0.10-0.45% Si, and optionally 0.20-0.70% Ni, 0.10-0.80% Cr, and 0.02-0.10% V. The heat treatment consists of surface quenching from above the austenitization temperature by means of a fluid, the heat remaining in the product being sufficient to temper the martensite and/or bainite in the quenched surface.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 17.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of manufacturing a rolled steel product having an elastic limit in the range from about 500 to about 1200 MPa, the method comprising subjecting a rolled steel product to intense cooling from above its austenitization temperature in such a way that at least part of the surface of the product is subjected to martensitic and/or bainitic quenching while the remainder of the product stays at a temperature sufficient to allow tempering of the quenched surface to occur subsequently by conduction of heat from the said remainder to the quenched surface, the rolled steel product containing 0.10
- Claim 2Depends on #1
A method as claimed in claim 1, in which the rolled steel product is a hot rolled product emerging from a finishing stand of a hot rolling mill.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗