Method of producing ethylene-vinyl alcohol copolymer film
Abstract
An ethylene-vinylalcohol copolymer film is prepared by biaxially or multiaxially stretching a nonstretched ethylene-vinylalcohol polymer film having a moisture content of not more than 3.5%, said ethylenevinyl alcohol copolymer having an ethylene content of 20 to 55 mole % and a saponification degree of not less than 96 mole % and said stretching being conducted within a temperature range of 50 DEG to 150 DEG C. to such an extent that the film is expanded to an area 4 to 20 times the original area.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 16.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of producing an ethylene-vinyl alcohol copolymer film, which comprises: biaxially or multiaxially stretching a nonstretched ethylene-vinylalcohol polymer film having a moisture content of not more than 3.5%, said ethylene-vinyl alcohol copolymer having an ethylene content of 20 to 55 mole % and a saponification degree of not less than 96 mole %, and said stretching being conducted within a temperature range of 50° to 150° C. to such an extent that the film is expanded to an area 4 to 20 times the original area.
- Claim 2Depends on #1
The method of claim 1, wherein the ethylene-vinyl alcohol copolymer has an ethylene content of 30 to 45 mole %.
- Claim 3Depends on #1
The method of claim 1, wherein the ethylene-vinyl alcohol copolymer has a saponification degree of not less than 98 mole%.