Patents
US 4,292,143 A#22859447 Most CitedExpiredUnited States (USPTO)Utility

Method of making sintered plaque nickel electrodes

4Forward Citations (#22859447 Global)
0.1/yrCitation Velocity (#46548603 Global)
2.15Citation PageRank (#12905636 Global)
3Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The improved method of the invention comprises electrochemically depositing nickel hydroxide into the pores of a clean sintered nickel plaque cathode from heated aqueous electrolyte at acid pH in a treating zone containing an anode, while minimizing corrosion of the plaque. The electrochemical deposition is continued only until a loading level of about 2 grams per cubic centimeter of void volume in the plaque is obtained. This is in order to avoid thickening, swelling and stressing of the plaque. The method is carried out without the need for a wetting agent in the electrolyte. The plaque should be sufficiently clean so as to be readily wetted throughout by the electrolyte. Such a clean condition can be produced by heating the plaque to at least about 700° C. Plaque corrosion is minimized by polarizing the plaque cathode as by the use of a sacrificial cadmium cathode. Plaque corrosion can also be minimized by maintaining an electric current in the electrolyte whenever the plaque is present therein. It is preferred to carry out the deposition while applying a substantially constant level of current to the electrodes. Loading levels of nickel hydroxide in excess of 7.7 ampere hours p

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 4.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An improved single step method of making sintered plaque nickel electrodes, said method comprising the single step of uniformly electrochemically depositing nickel hydroxide from a a heated aqueous alcohol-free electrolyte at a substantially constant current and a current density not in excess of about 1 A/in 2 (2.2 A/cc of void volume) into the pores of a clean sintered nickel plaque cathode at acid pH in a treating zone containing an anode, the deposition being continued only until the loading level of said nickel hydroxide throughout said sintered nickel plaque electrode reaches a uniform

  2. Claim 2Independent Claim

    The improved method of cla

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Journal of the Electrochemical Society, vol. 94, _Jul.-Dec. 1948, pp. 289-299.