Piezoelectric and pyroelectric film and method for preparing the film
Abstract
A piezoelectric and pyroelectric film made from a resin composition of polymer of vinylidene fluoride, which is characterized by an index of birefringence of larger than 3×10 -3 and a ratio of d 31 /d 32 of 0.3 to 3.0, and which may be prepared by further stretching a biaxially stretched film made from the above-mentioned resin composition at a temperature lower than the temperature of the biaxially stretching by more than 20° C. before or at the same time of a treatment for orientation polarization of the film.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 45.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for preparing a piezoelectric and pyroelectric film comprising the steps of, biaxially stretching a film made from a resin composition of a polymer of vinylidene fluoride; additionally stretching the thus obtained biaxially stretched film at a temperature of lower than the crystallizing temperature of said resin composition, which additional stretching temperature is lower than the temperature at the biaxially stretching by more than 20° C. and is higher than the secondary transition temperature of said resin composition; and at the same time or after the additional stretching p
- Claim 2Depends on #1
The method according to claim 1, wherein said resin composition comprises a homopolymer or copolymer of vinylidene fluoride.
- Claim 3Depends on #1
The method according to claim 1, wherein th
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗