Metals such as nickel, vanadium and iron contaminating a cracking catalyst are passivated by contacting the cracking catalyst under elevated temperature conditions with tungsten and compounds of tungsten.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 10.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A modified cracking catalyst obtained by contacting a zeolite-modified silica-alumina cracking catalyst on which a deactivating amount of at least one metal selected from the group consisting of nickel, iron, and vanadium has been deposited and at least one passivating material selected from tungsten and compounds of tungsten under elevated temperature conditions in an amount such as to add about 0.05 to 2 weight percent tungsten based on the weight of the untreated catalyst.
- Claim 2Depends on #1
A catalyst in accordance with claim 1 obtained by contacting the cracking catalyst with the passivating material at temperatures in the range of about 800° F. (427° C.) to about 1500° F. (816° C.) and under reducing conditions.
- Claim 3Depends on #1
A catalyst in accordance with claim 1 obtained by contacting the cracking catalyst with tungsten at temperatures in th