Method for the production of sintered powder ferrous metal preform

10Forward Citations (#9771579 Global)
0.2/yrCitation Velocity (#31093644 Global)
5.48Citation PageRank (#2854295 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for the production of sintered powder metal preform employing a novel reduction step. As-water-atomized ferrous metal particles are coated by phenol resins by adding said phenol resins to said ferrous metal particles after heating the metal particles to about 130° C. to 150° C. Resin coated ferrous metal particles are then filled in a mold and compacted under high pressure to produce a compacted green preform sufficient to ensure adequate strength for handling after pressing. The green preform is then heated to a reduction temperature within the range of about 1100° C. to 1250° C. for a time sufficient to achieve reduction of said green preform.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 10.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for the production of sintered powder ferrous metal preforms comprising the steps of; heating said ferrous metal particles to a temperature of about 130° C. to 150° C.; coating finely divided ferrous metal particles with thermoplastic phenol resins having an effective carbon content of 10 to 40 percent by adding said phenol resins to said ferrous metal particles, wherein said phenol resins are present from about 1.0 to 7.0 percent of the total mixture; cooling said resin coated ferrous metal particles by blowing cooling air thereto; packing a mold with said resin coated ferrous me