Electroplating of nickel-iron alloys for uniformity of nickel/iron ratio using a low density plating current

42Forward Citations (#1271887 Global)
0.9/yrCitation Velocity (#7645562 Global)
7.89Citation PageRank (#1570731 Global)
11Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Electroplating nickel-iron alloys onto objects having complex topographical shapes with projections and hollows such as upper pole pieces of thin film magnetic recording heads has been found to yield a substantial variation in nickel-iron alloy composition from point to point within a single pattern. Providing a low total dischargeable ion concentration in the bath is helpful to reduce such variations when plating in the 80:20 Ni:Fe alloy range. That is, it is desirable to use a low value of Fe ++ and Ni ++ ion concentrations and a relatively low current density to operate at the relatively flat peak of the curve of the iron percentage in the plated alloy vs. current density curve. The curve can be raised or lowered by increasing or decreasing the total dischargeable ion concentration respectively for a given Ni ++ /Fe ++ ion ratio. The preferred Fe ++ ion concentration range for Ni:Fe alloy ratio near 80:20 is about 0.15-0.3 g/l for a range of 10-14 g/l of Ni ++ ion in a solution with a pH of about 3, a temperature of about 20°-35° C. where the Ni ++ /Fe ++ ratio in the solution ranges from about 45 to 1 to about 70 to 1. Preferably, an electrolyte for reducing pitting such as 0-1

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 42.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A nickel-iron electroplating method for plating NiFe alloy onto a substrate with a relatively high degree of uniformity of magnetic nickel-iron alloy composition over a range of plating current densities comprising, an aqueous plating bath solution at a temperature in the range from about 20° C. to about 35° C., placing a substrate with a complex topographical shape in said plating bath solution, employing a constant current plating density from about 2 milliamperes per centimeter squared to about 12 milliamperes per centimeter squared, said plating bath solution having ferrous ion concent