Process for preparation of a polymeric piezo-electric material and material prepared by said process

28Forward Citations (#2462655 Global)
0.6/yrCitation Velocity (#12753122 Global)
17.23Citation PageRank (#428434 Global)
4Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A process for preparation of a polymeric piezo-electric material and material prepared by said process are described, wherein said process comprises polarizing a polymeric piezo-electric material by a polarization treatment which comprises cooling a vinylidene fluoride-trifluoroethylene copolymer from a temperature higher than the phase transition temperature of said copolymer which exists between room temperature and the melting point of said copolymer, and either maintaining the temperature range at which said copolymer possesses a maximum in dielectric constant occurs, or cooling gradually through said temperature range, while applying an electric field at least within said temperature range.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 28.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a polymeric piezo-electric material by a polarization treatment which comprises cooling a vinylidene fluoride-trifluoroethylene copolymer from a temperature higher than the phase transition temperature of said copolymer which exists between room temperature and the melting point of said copolymer and either maintaining the temperature within the temperature range where a maximum of dielectric constant occurs, or cooling gradually through said temperature range, while applying an electric field at least within said temperature range.

  2. Claim 2Depends on #1

    A process for preparing a polymeric piezo-electric material according to claim 1 which comprises applying electric field of from about 100 to 600 KV/cm, at a temperature range at least as high as the temperature range at which a maximum of dielectric constant occurs.