Abstract

A process for the preparation of a rubber-modified thermoplastic resin, which comprises treating an ethylene-propylene-non-conjugated diene copolymer rubber with a peroxide in a hydrocarbon or halogenated hydrocarbon solvent to obtain a rubber solution with a rubber gelation degree of not more than 5% and containing substantially no unreacted peroxide, adding to this rubber solution a vinyl monomer consisting of an aromatic alkenyl compound and a polar vinyl compound, and heating the resulting mixture to graft-copolymerize the monomer on the rubber. The resin obtained according to this process is free of fish eyes and proof against delamination of shaped article and has excellent mechanical properties, excellent appearance when shaped and high weather resistance.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 4.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for the preparation of a rubber-modified thermoplastic resin, which comprises: treating an ethylene-proylene-non-conjugated diene copolymer rubber with a peroxide in a hydrocarbon or halogenated hydrocarbon solvent to obtain a rubber solution having a rubber gelation degree of not more than 5% and containing substantially no unreacted peroxide; adding to said rubber solution without isolating the treated copolymer a vinyl monomer mixture consisting of an aromatic alkenyl compound and a polar vinyl compound; and heating the resulting mixture in the substantial absence of a polymeriz

  2. Claim 2Depends on #1

    The process according to claim 1, wherein the peroxide is used in an amount of 0.1-10 parts by weight per 100 parts by weight of the rubber.

  3. Claim 3Independent Claim