Electrohydrodynamic spraying to produce ultrafine particles
Abstract
Amorphous or microcrystalline alloy powder is prepared by the rapid quenching of ultrafine metallic spheroids generated from the molten metal state. The molten metal droplets are formed when an intense electric field (10 5 V/cm) is applied to the surface of liquid metal held in a suitable container. The interactions between the intense electric field and liquid surface tension disrupts the metal surface, resulting in a beam of positively charged droplets. The liquid metal spheres generated by this electrohydrodynamic process are subsequently cooled by radiative heat transfer. Rapid cooling of the droplets may be accomplished by heat transfer to a low pressure gas by free molecular heat conductivity. Quenching rates exceeding 10 6 °K./sec are possible using this technique. Thin film coatings are prepared by electrohydrodynamically spraying a beam of charged droplets against a target (substrate). The target can be electrically controlled to effect the charged particles impact. The materials to be sprayed electrodynamically can be varied in both throughput and species such that a target can have multimaterial layers being deposited coincidentally or sequentially. The ultra small dropl
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 174.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of forming high melting temperature metal alloys in the form of ultrafine particles ranging in size from sub-micron to about 100 microns by electrohydrodynamic spraying which comprises: liquefying the metal alloy; pneumatically feeding the molten metal alloy to a capillary nozzle to form a liquid meniscus at the tip of the nozzle; applying a positive electric field to the molten metal alloy to create electrostatic forces which are high enough to overcome the surface tension of the liquid meniscus to thereby generate a beam of positively charged ultrafine droplets of said metal all
- Claim 2Depends on #1
The method of claim 1 which is carried out in a vacuum chamber evacuated to at most about 0.5 atmospheres.
- Claim 3Independent Claim
The
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 174 total)
References Cited — Backward Prior Art (17)
Non-Patent Literature (1)
- "Production of Ions by Electrohydrodynamic Spraying Techniques", Swatik, D. S. and Hendricks, C. D., AIAA Journal, vol. 6, No. 8, pp. 1596-1597, Aug. 1968.