Patents
US 4,255,409 A#37652131 Most CitedExpiredUnited States (USPTO)Utility

Process for producing acicular goethite

2Forward Citations (#37652131 Global)
0.0/yrCitation Velocity (#55546475 Global)
1.09Citation PageRank (#36821068 Global)
4Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An alkali hydroxide is added to an aqueous solution of ferrous salt to form a precipitate and a part of the solution is separated to control a ratio of an anion to a ferrous component to less than 1 and the ferrous component is oxidized to acicular goethite with an alkali metal chlorate such as potassium chlorate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for producing an acicular goethite comprising: adjusting the pH of an aqueous solution of a ferrous salt to a value higher than 11; allowing a precipitate of ferrous hydroxide to form; adjusting the ratio of the anion of the ferrous salt to the ferrous hydroxide to 0.1 to 0.5 by separating a portion of the supernatant from said precipitate; and oxidizing the precipitate with an alkali metal chlorate at a temperature lower than 80° C.

  2. Claim 2Depends on #1

    The process according to claim 1, wherein the pH of the aqueous solution of a ferrous salt is adjusted to a value higher than 11 by adding an alkali metal hydroxide or carbonate thereto.

  3. Claim 3Depends on #1

    The process according to claim 1, wherein the ferrous salt is selected from the group consisting of ferrous sulfate, ferrous nitrate, ferrous chloride, ferrous phosphate and ferrous ac

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗