US 4,243,554 A#186292 Most CitedExpiredUnited States (USPTO)Utility

Molybdenum disulfide catalyst and the preparation thereof

112Forward Citations (#186292 Global)
2.5/yrCitation Velocity (#1347896 Global)
23.66Citation PageRank (#252213 Global)
11Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

High surface area molybdenum disulfide, MoS2, is produced by the thermal decomposition of selected ammonium thiomolybdate salts at temperatures of about 300 DEG -800 DEG C., with said salts being heated to decomposition temperature at a rate in excess of about 15 DEG C./min., e.g., about 20 DEG -30 DEG C./min., in an essentially oxygen-free atmosphere. The product molybdenum disulfide has superior catalytic properties for the water gas shift and methanation reactions compared with conventional MoS2. The stability of the catalyst is enhanced by decomposing the thiomolybdate salt in admixture with an inert, preformed particulate diluent or by bulk doping said salt with tungsten or vanadium prior to decomposition of the salt. The molybdenum disulfide of the invention also has desirable properties for use in catalyzed hydrogenation and hydrotreating reactions, i.e., hydrodenitrogenation and hydrodesulfurization reactions, particularly when employed in nickel or cobalt-promoted form.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 112.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for the production of improved, sulfur resistant catalysts comprising thermally decomposing an ammonium salt of molybdenum-sulfur cluster anions or an ammonium thiomolybdate salt having the formula (NH 4 ) 2 [MoO x S 4-x ], where x is from about 0.8 to about 2.2, at a decomposition temperature of from about 300° C. to about 800° C., said salt being heated to the decomposition temperature rapidly at a rate in excess of about 15° C./min. in an essentially oxygen-free atmosphere, said salt decomposing at said temperature to form a high surface area, bulk molybdenum disulfide, MoS 2 ,

  2. Claim 2Depends on #1

    The process of claim 1 in which said salt is decomposed at a temperature of from ab

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Thermal Decomp. of (NH.sub.4).sub.2 MoO.sub.2 S.sub.2 ", T. P. Prasad et al., J. of Inorg. Nucl. Chem., 1973, vol. 35, pp. 1895-1904.
  • "Thermal Decomp. of (NH4)2 MoO2 S2 ", T. P. Prasad et al., J. of Inorg. Nucl. Chem., 1973, vol. 35, pp. 1895-1904.
  • Angew, Chem. Int. Ed. Engl. 17, 279, (1978).
  • Angew, Chem. Int. Ed. Engl. 17, 535, (1978).
  • Mills & Steffgen, Cat. Rev. 8,159, (1973).