Abstract

A method is described for making a shaped silicon carbide-silicon matrix composite. A confined carbon fiber preform is infiltrated with sufficient molten silicon metal at a temperature in the range of from about 1400° C. to about 1800° C. in an inert atmosphere or vacuum. Silicon carbide powder can also be incorporated in the preform structure.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 33.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A shaped ceramic consisting essentially of axially aligned silicon carbide crystals in a silicon metal matrix having from about 4% by weight to about 30% by weight of carbon in a chemically combined form or as a mixture of chemically combined carbon and elemental carbon, said shaped ceramic exhibiting a density of about 2.3 to 3.0 grams/cc, a permanent elastic strain when measured at about 1000° C. of from about 0% to about 6%, and an elastic modulus of from about 30×10 6 psi to 60×10 6 psi.

  2. Claim 2Depends on #1

    A shaped ceramic as in claim 1 where the axially aligned silicon carbide crystals have a general parallel relationship.

  3. Claim 3Depends on #1

    A shaped ceramic as in claim 1 which further includes other silicon carbide crystals dispersed in the silicon metal matrix.