Patents
US 4,239,796 A#1915563 Most CitedExpiredUnited States (USPTO)Utility

In-mold coating of structural foams and resultant product

33Forward Citations (#1915563 Global)
0.7/yrCitation Velocity (#10515837 Global)
6.98Citation PageRank (#1922495 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method is disclosed comprising in-mold coating a structural foam part made from a thermoplastic aromatic polycarbonate resin or a thermoplastic ABS polymer resin with a thermosetting in-mold coating composition at a pressure of from about 25 to 50 p.s.i. and at a temperature not in excess of about 200° F. for from about 1 to 10 minutes, preferably for from about 1 to 3 minutes, to provide hard, smooth and adherent coatings, said thermosetting in-mold coating composition comprising an ethylenically unsaturated polyester resin and an ethylenically unsaturated monomer(s) catalyzed with an organic perioxide initiator including an accelerator for the initiator.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 33.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    The method which comprises in-mold coating a molded structural foam part of a thermoplastic resin selected from the group consisting of an aromatic polycarbonate resin and an ABS polymer resin with a thermosetting in-mold coating composition and heating said composition at a temperature not in excess of about 200° F. for from about 1 to 10 minutes at a pressure of from about 25 to 50 p.s.i. to cure the same to form an adherent, hard and glossy coating, said in-mold coating composition comprising (a) an ethylenically unsaturated polyester having an average molecular weight of from about 1,000 t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗