Production of fine metal powders
Abstract
Metal particles which are ductile at ambient temperature can be comminuted by being passed through a first impact mill at ambient temperature to increase their length to thickness ratio, embrittled, and then comminuted in a second impact mill.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 13.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of comminuting oversize ductile metal powder particles produced by water or gas atomization comprising the steps of impacting the particles to increase their length to thickness ratio thus producing generally elongated flattened particles, cooling the elongated particles to a temperature at which the elongated particles become embrittled and further comminuting the embrittled particles to produce relatively fine powder.
- Claim 2Depends on #1
A method according to claim 1, wherein the ductile metal powder particles are impacted within a vibratory ball mill to produce length to thickness ratios in excess of 10.1.
- Claim 3Depends on #1, #2
A method according to claim 1 or 2, wherein said impacted particles are cooled to below their embrittlement temperature and then comminuted in a rotary impact mill.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (13 of 13 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,015,780 A | Powder forming | 1977 | 14 |
| US 4,018,633 A | Cryogenic metal chip reclamation | 1977 | 18 |