Anaerobic curing adhesive composition and process for making same
Abstract
Storage-stable anaerobic curing adhesive compositions useful as anaerobic adhesives and sealants are prepared by first mixing a polymerizable acrylate ester monomer, an inhibitor for free radical polymerization, a chelator, and at least an effective amount of an accelerator system consisting of an organic cyclic sulfimide, preferably saccharin, and an aromatic tertiary amine. The resultant homogeneous mixture is thereafter heated at a temperature of about 45°-100° C. for a period of time sufficient to provide the composition with anaerobic curing properties and a specified minimum amount of active oxygen. In one embodiment, the mixture is stirred at a temperature of 45°-70° C. for 10-24 hours. In another embodiment, the mixture is maintained at an elevated temperature without stirring.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 21.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An improved process for preparing a storage-stable adhesive composition capable of curing in the absence of air which process comprises: (a) forming a homogeneous mixture consisting essentially of a polymerizable acrylate ester monomer, from 0.0001 to 0.1% by weight, based on monomer, of an inhibitor for free radical polymerization, from 0.0001 to 0.1% by weight, based on total composition, of a soluble chelator having ligand atoms other than nitrogen ligand atoms of the ≦C=N-type, this amount being dependent on the chelator, and at least an effective amount of an accelerator system consisting
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 21 total)
References Cited — Backward Prior Art (3)
Non-Patent Literature (1)
- Lal et al, J. Pol. Sci., XXIV, pp. 75-84, (1957).