Method for forming activated alumina coating on refractory article and article thereby produced
Abstract
A mixture is prepared by mixing alumina sol and activated alumina which contains not less than 60 Wt % of delta-alumina. The mixture is thereafter coated on a relatively small specific surface area monolithic catalyst carrier. After being dried, the coated carrier is fired to give a high specific surface area catalyst carrier.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 27.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for forming a high surface area coating on the surface of a monolithic catalyst carrier, said method comprising the steps of: preparing a mixture containing not more than 20 parts by weight of alumina sol and one part by weight of activated alumina, said alumina sol containing 3 to 15 Wt % of alumina, said activated alumina containing not less than 60 Wt % of delta-alumina; coating said mixture onto the surface of the catalyst carrier; drying the coated catalyst carrier; and firing the coated catalyst carrier at a temperature in the range of 150° to 850° C. for a time in the ran
- Claim 2Depends on #1
A method as claimed in claim 1, in which said alumina sol is prepared by using alumina whose starting material is boehmite, and the s
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗