Size for forming glass fibers having a reduced tendency to give gumming deposits
Abstract
A method and composition are provided for producing an improved sized glass fiber strand that has a reduced tendency to form gummy deposits on fabrication machinery under high relative humidity conditions. The glass fiber strand is treated with a starch based forming size comprising about 50 to about 65 weight percent of the non-aqueous components of the composition being a starch containing cross-links that has been partially cooked along with a hydrogenated vegetable oil, or fatty triglyceride, cationic wetting agent, emulsifying agent, and water. The forming size composition can also contain a salt of a polyamino functional polyamide resin and a carboxylic acid and a wax and a coupling agent.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 12.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A sizing composition to treat glass fibers to produce a glass fiber strand with a reduced tendency to form gummy deposits on fabrication machinery under high relative humidity conditions, comprising in weight percent based on the non-aqueous components in the sizing composition: (a) about 50 to about 65 of a starch having cross-links that has been partially cooked at a temperature in the range of about 220° F. to about 250° F. in a jet cooker at a pressure of 90 to about 110 psi and cooled to around 190° F., (b) 4 to 52 percent of the salt of a polyaminofunctional polyamide resin, said polya
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗