Patents
US 4,200,602 A#40493842 Most CitedExpiredUnited States (USPTO)Utility

Method for producing filaments of high tenacity

2Forward Citations (#40493842 Global)
0.0/yrCitation Velocity (#55685092 Global)
1.00Citation PageRank (#41686341 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A molten polymer is extruded through at least one orifice to produce a filament which is immediately cooled to a temperature below its glass transition temperature by contacting the filament with a gas having a temperature ranging from about +10 DEG C. to about -20 DEG C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method comprising extruding a molten polymer through at least one orifice to produce a filament and immediately cooling said filament to a temperature below its glass transition temperature by contacting said filament with a gas having a temperature ranging from about -20° C. to about 10° C., said polymer is the condensation product of 5-methyl-1,9-nonanediamine and terephthalic acid wherein the filament is heated and drawn at a temperature ranging from about 2° C. to about 40° C. below the glass transition temperature of the polymer.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the temperature of the gas ranges from about -10° C. to about 0° C.

  3. Claim 3Depends on #1

    The method of claim 1 wherein the gas is air.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)