Alloys for gettering moisture and reactive gases
Abstract
Alloys reacting with water, water vapor and reactive gases at temperatures in the range of about 200° to about 650° C. have the essential components of nickel, titanium and zirconium. The alloys can be made by arc melting zirconium, nickel and titanium and can be formed into sheet or foil by inert-atmosphere hot rolling. The alloys can also be made by plating nickel on a sheet of zirconium-titanium alloy and then conducting a diffusion process by heating the plated alloy in vacuum.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 15.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A getter alloy having the essential components of zirconium, nickel and titanium comprised of about 4 weight percent nickel, about 11 weight percent titanium, and the balance being zirconium, said alloy being capable of reacting with water, water vapor, hydrogen, carbon monoxide, carbon dioxide, oxygen and hydrocarbons.
- Claim 2Independent Claim
A getter alloy having the essential components of zirconium, nickel and titanium comprised of about 12 weight percent nickel, about 13 weight percent titanium and the balance being zirconium, said alloy being capable of reacting with water, water vapor, hydrogen, carbon monoxide, carbon dioxide, oxygen and hydrocarbons.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 15 total)
References Cited — Backward Prior Art (3)
Non-Patent Literature (4)
- Nuclear Sci. Abstracts, vol. 19, #13, Jul. 15, 1965, No. 24982.
- Nuclear Sci. Abstracts, vol. 19, #17, Sep. 15, 1965, No. 32696.
- Nuclear Sci. Abstracts, vol. 22, #11, Jun. 15, 1968, No. 21659.
- Nuclear Sci. Abstracts, vol. 24. #16, Aug. 31, 1970, No. 32345.