Method for producing polylaurolactam powder compositions for the coating of metals at high temperatues

4Forward Citations (#22526218 Global)
0.1/yrCitation Velocity (#46435522 Global)
5.69Citation PageRank (#2682662 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Polylaurolactam powder coating compositions for the coating of metals at high temperatures are obtained by grinding low molecular weight and brittle polylaurolactam with subsequent condensation by heating of the powder to temperatures of below its melting point. A. For the production of pigment free polylaurolactam powders, the low molecular weight granules are ground at temperatures of between 0° and 45° C. which have a relative viscosity of between 1.25 and 1.45 (measured in a 0.5 percent mecresol solution at 25° C.) and have been produced by the polymerization of laurolactam in the presence of 2-10 percent by weight of water, 0.3-0.7 percent by weight of phosphoric acid at temperatures of between 265° and 300° C. in the absence of chain stabilizers under internal pressure, with subsequent granulating, and extraction between 25° and 70° C. with methanol or ethanol. The subsequent condensation is conducted at temperatures of between 140° C. and below the melting point of the polyamide to relative viscosity value of between 1.55 and 1.65; and finally the powders obtained are brought to a particle size distribution of between greater than 60 and less than 350 microns. B. For the pro

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing polylaurolactam powders comprising: (a) polymerizing laurolactam in the presence of about 2 to 10 percent by weight of water, based on said laurolactam, about 0.3 to 0.7 percent by weight of phosphoric acid, based on said laurolactam and at a temperature of about 265° to 300° C. in the absence of chain stabilizers under an internal pressure of about 14 to 25 bars to a polylaurolactam having a relative viscosity of about 1.25 to 1.45 measured in a 0.5 percent meta-cresol solution at 25° C.; (b) granulating said polylaurolactam of (a); (c) extracting said granulated pol

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • "Eveil de Berney", French Newspaper, Jan. 22, 1970, p. 3.