Poly(ethylene terephthalate) filaments of enhanced dyeability, low boil-off shrinkage (even in as-spun condition), good thermal stability over a large temperature range; and useful as texturing feed yarns and/or as hard yarns requiring no further drawing are prepared by spinning at extremely high speeds, and are characterized by a long period spacing above 300 A in their as-spun condition, and, whether in as-spun condition or after heat-treatment, by a low skin-core value as measured by a differential birefringence in relation to their stress measured at 20% extension (which correlates approximately with the spinning speed), a large crystal size, and low amorphous orientation. The continuous filament yarns may be draw-textured to provide textured yarns which also show enhanced dyeability. The staple fiber yarns also have very useful properties as compared with conventional staple yarns. A preferred process of spinning at these extremely high speeds is characterized by the use of a spinneret with capillary-dimensions that produce high shear as the polyester is extruded, and is applicable also to copolyesters, whose filaments show a similar low skin-core in relation to their stress a

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 73.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    In a process for melt-spinning ethylene terephthalate polyester and cooling in the atmosphere to solidify as filaments with a low differential birefringence between the surface and the core of such filaments, the improvement, when withdrawing the filaments at a speed (V in yards/minute) of at least about 5500 yards/minute, wherein the polymer temperature (T p ), measured (in °C.) in the filter pack at a point 50-100 mils above the center of the spinneret plate, is maintained above a minimum value depending on an exponential of the speed V and a function of the length (L) and diameter (D) (in m

  2. Claim 2Depends on #1

    A process according to claim 1, wherein the speed (V) is at least about 7000 yards/minute.

  3. Claim 3Independent Claim

    A proc