Method and apparatus for frit-sealing high temperature CRT faceplate to conventional CRT envelope

5Forward Citations (#19427965 Global)
0.1/yrCitation Velocity (#43499303 Global)
2.10Citation PageRank (#13420534 Global)
11Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A cathode ray tube has an envelope comprised of a first glass and a faceplate comprised of a second glass, both glasses having different thermal coefficients of expansion. The envelope and faceplate are joined by a cylindrical, stress-absorbing glass member flame-sealed at one end to the envelope and frit-sealed at the other end to the faceplate. Importantly, the thermal coefficient of expansion of the stress-absorbing member is less than the coefficients of either the envelope or the faceplate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 5.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of joining a first glass member having a first thermal coefficient of expansion to a second glass member having a second thermal coefficient of expansion, said method comprising the steps of: joining one end of a third glass member having a third thermal coefficient of expansion to said first member and also joining the other end of said third member to said second member, said third member extending lengthwise between said first and second members and acting as an intermediate stress-absorber and having a thermal coefficient of expansion which is less than both said first and said se

  2. Claim 2Depends on #1

    The method according to claim 1 wherein said joining step includes: flame-sealing said fir

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • "Material Information" (Corning Code 1720), Sep. 1972, by Corning Glass Works.
  • "Material Information" (Corning code 7052), Aug. 1977, by Corning Glass Ws.
  • "Material Information" (Corning code 7052), Aug. 1977, by Corning Glass Ws.