Oxygen electrode rejuvenation methods
Abstract
Disclosed are methods for rejuvenation of oxygen electrodes which maximize the power efficiency available from such oxygen electrodes while minimizing the voltage necessary to operate such oxygen electrodes over extended periods of time. These methods include in situ and out of cell techniques using hot water washing followed by air drying and dilute acid washing followed by air drying.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 11.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for rejuvenation of a failed oxygen electrode which has been in use in a chlor-alkali electrolytic cell comprising the steps of: washing the oxygen electrode with a solution selected from the group consisting of water or a dilute acid solution; drying the oxygen electrode with a gaseous substance at a temperature in the range of 200° to 360° C.; and subsequent to the drying step, applying a pressure in the range of 1000 to 3000 pounds per square inch for a time period in the range of 30 to 180 seconds.
- Claim 2Depends on #1
A method according to claim 1 wherein the drying gaseous substance is air.
- Claim 3Depends on #2
A method according to claim 2 wherein said washing step consists essentially of: a first soaking of the oxygen electrode in deionized water for a period in excess of 24 hours; a second washing of the oxygen electrode in a sol