Patents
US 4,180,418 A#7958889 Most CitedExpiredUnited States (USPTO)Utility

Method of making a steel wire adapted for cold drawing

12Forward Citations (#7958889 Global)
0.3/yrCitation Velocity (#27880233 Global)
4.66Citation PageRank (#3713281 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A steel wire after coming from the mill is brought to a temperature between 850° and 910° C. This is followed by multi-stage water-cooling of the wire in such a manner that the surface of the wire is cooled to below the martensite start temperature while austenite is retained in the core of the wire. The heat retained in the core of the wire serves to partially temper the martensite formed at the surface of the wire. The wire is coiled while the temperature remains substantially constant so that the retained austenite in the core of the wire undergoes an isothermal transformation to fine pearlite. The heat of transformation serves to complete tempering of the martensite. After coiling, the wire is air-cooled to room temperature. The final wire exhibits a structure consisting of an outer layer of tempered martensite and a core of fine pearlite. This structure imparts excellent cold-working characteristics to the wire.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 12.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process of making a steel wire of high strength and good cold drawing properties, the said process comprising (a) after hot rolling the wire bringing it to a temperature between about 850° and 910° C. so as to obtain a fine grain austenite structure in the wire; (b) thereafter quenching the wire to cool it to a temperature of about 500° C.; (c) coiling the wire after said quench and finally cooling it to room temperature, the said quench being carried out in a manner that a transformation to martensite occurs which is limited to the outer surface of the wire not to exceed 33 percent of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗