Abstract

Reinforced plastic pipe is made at high rates using a wiper to remove resin from the surface of the rovings after they are applied to a rotating mandrel. The wiper leaves an optimum surface layer of resin on the rovings. For small diameter pipe, production rates are further increased by rotating the mandrel above its first critical speed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 15.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    In a method for manufacturing plastic pipe reinforced with fibrous rovings comprising the steps of coating the rovings with a fluid resin, and winding a rotating mandrel with the resin coated rovings, the improvement which comprises the step of contacting the wound rovings with at least one filament segment curved around a portion of the wound pipe, and moving the filament segment longitudinally along the mandrel during the winding as the mandrel is rotated to wipe resin from the wound rovings to leave a substantially uniform surface layer of resin on the rovings, the layer being sufficiently

  2. Claim 2Depends on #1

    A method as claimed in claim 1 wherein the mandrel is rotated faster than its first critical speed.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Eshleman, "Flexible Rotor-Bearing System Dynamics, Critical Speeds and Response of Flexible Rotor Systems," 1972, The American Society of Mechanical Engineers, pp. 1 & 30.