Relief plates from polymer with terminal unsaturation
Abstract
It has been found that excellent quality photopolymer printing plates having hardness, flexibility, resilience, abrasion resistance and resistance to alcohol-based inks can be prepared from photopolymer compositions comprising a liquid polymer containing at least two terminal olefin groups attached to the polymer through a combination of at least two ether, thioether, ester, keto or amide groups, from about 1 to about 50% by weight based on the polymer of at least one ethylenically unsaturated monomer, from about 0.1 to about 10% by weight of a photoinitiator and about 0.01 to about 2% of a stabilizer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 23.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
The process of making a printing relief which comprises (1) admixing (a) a liquid terminal olefinically unsaturated linear polymer having a molecular weight in the range of from 1,000 to 20,000 selected from polymers having the structure ##STR18## where X is selected from --O--, --S--, ##STR19## and --NH-- groups; Y is selected from --O--CH 2 --CH═CH 2 and ##STR20## R' is selected from --H and --CH 3 groups; Z is selected from ##STR21## and ##STR22## where R" is selected from --H, --CH 3 and ##STR23## and P is a polymer residue selected from homopolymers of butadiene, isoprene, chl
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗