Process for the production of a tungsten carbide catalyst by carburization of tungsten oxides
Abstract
A process for the production of a tungsten carbide catalyst by carburization of tungsten oxides, comprises, directing a mixture of carbon monoxide and carbon dioxide over tungsten oxide while heating it in a heated reactor at a heating rate and gas flow rate such that the reduction of the tungsten oxide occurs more slowly than the diffusion of the carbon into the tungsten and into tungsten carbide which is formed during the reaction with the diffusion being faster than the separation of carbon from the gaseous phase according to the rate of adjustment of the Boudouard equilibrium. The carbon monoxide is charged at a rate of 560 1tr/h and the carbon dioxide is charged at a rate of 40 1tr/h and, after a reactor containing the sample of tungstic acid is positioned in a closed reactor, the reactor is flushed with the gases for around ten minutes and then placed into a muffle furnace. The reactor is heated to a temperature of 670° C. in the furnace and the temperature is then reduced to a reaction temperature of 620° C. First, all of the water is eliminated, and then there is a reduction of the tungsten oxides and a diffusion of the carbon into tungsten or into tungsten carbide which is
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 14.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for the production of a tungsten carbide catalyst by carburizing tungsten oxide at high temperatures while using a gas mixture of carbon monoxide and carbon dioxide acting on a reactant placed in a heated reactor comprising directing a mixture of carbon monoxide and carbon dioxide over the tungsten oxide while heating the tungsten oxide in a heated reactor maintained at a temperature in between from 590°-680° C. and for a reaction time of between 10 and 16 hours with a flow of carbon monoxide in the range of from 200 to 800 ltr/hr and with a flow of carbon dioxide of from 20-40 ltr/h
- Claim 2Independent Claim
A process according to cla
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (14 of 14 total)
References Cited — Backward Prior Art (3)
Non-Patent Literature (1)
- Micron (1975) vol. 6, No. 3-4; pp. 147-152 (Pergamon Press) "Characterization of Ultra-High Surface Area Tungsten Carbide", A. E. Forwalt et al.