Patents
US 4,159,926 A#8572139 Most CitedExpiredUnited States (USPTO)Utility

Nickel plating

12Forward Citations (#8572139 Global)
0.3/yrCitation Velocity (#27973152 Global)
2.00Citation PageRank (#14552830 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A nickel electroplating bath comprises in aqueous solution at a pH of from 4 to 7, nickel ions at a Molar concentration of at least 0.25, chloride ions at a Molar concentration of at least 0.25, and a weak complexant for the nickel selected from formate, acetate, citrate, glutamate, anions and lactones of sugar acids and anions and lactones of acids having the formula X(C n H 2n )COOH where X is OH or NH 2 and n is 1 to 5, preferably 1 to 2, present at a Molar concentration of from 0.5 to 4.0 times that of the nickel. These baths have good throwing power and can be operated at convenient temperatures and pH values and at lower nickel ion concentrations than hitherto.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 12.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of electrodepositing nickel on an object having a metallic surface, which method comprises providing a nickel electroplating bath consisting essentially of, in aqueous solution at a pH of from 4.0 - 6.5: ______________________________________ Constituent Molar Concentration ______________________________________ Nickel ions at least 0.25 Chloride at least 0.25 Sulphate (optional) less than 0.25 ______________________________________ and a weak complexant for the nickel selected

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • H. Koretzky, IBM Tech. Disclosure Bulletin, p. 1634, vol. 9, No. 11, Apr. 1967.