Patents
US 4,159,918 A#30304532 Most CitedExpiredUnited States (USPTO)Utility

Method of manufacturing a compound steel material of a high corrosion resistance

3Forward Citations (#30304532 Global)
0.1/yrCitation Velocity (#51751319 Global)
1.23Citation PageRank (#30949265 Global)
4Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A compound steel material of high corrosion resistance is manufactured by alloying a carbon steel carrier material having a carbon content of at most 0.20C and of at least 0.04C with a carbide and nitride forming substance, compounding the alloyed carrier material with a ferritic chromium steel material of normal carbon content, followed by hot-rolling the compound steel material to a hot rolled strip or sheet which is then annealed at a temperature and for a time period sufficient for the carbon content of the ferritic chromium steel coating layer to be reduced to between 0.001 and 0.003% so as to increase the corrosion resistance of the chromium steel material to that of a superferritic material. After annealing, the sheet may be etched and surface-finished or cold-rolled, recrystallization annealed and thereafter surface-finished, such as temper-rolled. The ferritic chromium steel material has at most 0.1% of carbon prior to annealing. The carbide and nitride forming substance may be titanium whose content in the alloyed carrier material is preferably between 0.50% and 2.00%. The thickness of the ferritic chromium steel coating layer is between 50 and 500 μm, the annealing tempe

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a compound steel material having at least one chromium steel coating layer, comprising the steps of alloying a carbon steel carrier material with a carbide and nitride forming substance; compounding the alloyed carrier material with a chromium steel material of normal carbon content; hot-rolling the compound steel material to a sheet; and increasing the corrosion resistance of the chromium steel material of the sheet to that of a superferritic material, including annealing the compound steel material at a temperature and for a time period sufficient for the carbon con

  2. Claim 2Depends on #1

    A method as defined in claim 1, wherein the carbon content of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗