Process for the production of fiber-grade terephthalic acid
Abstract
Process for the preparation of fiber-grade terephthalic acid by continuously oxidizing paraxylene while vaporizing a portion of the contents of the reactor. Fiber-grade terephthalic acid is produced by maintaining (1) a temperature of at least 210° C., (2) a molecular oxygen content of the noncondensables in the vapor withdrawn from the reactor in the range 3.0-6.0%, (3) a water level of the contents of the oxidizer in the range 5.0-17.0%, (4) a mole ratio of sodium to cobalt plus manganese in the range 0.06-2.0 in the reactor, (5) a mole ratio of cobalt to manganese in the range 0.5-5.0 (6) an organic burn in the range 8.0-15.0 burn units and (7) a productivity in the range 0.45-1.45 pounds of terephthalic acid per minute per 100 pounds of reactor contents.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 211.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
In a process for the preparation of fiber-grade terephthalic acid comprising oxidizing paraxylene with a molecular oxygen containing gas in a reactor in the presence of a catalyst consisting essentially of cobalt, manganese, sodium and bromine and a solvent comprising a lower monocarboxylic acid wherein (1) the oxidation is conducted in the liquid phase, (2) a portion of the contents of the reactor is continuously vaporized, withdrawn from the reactor and at least a portion thereof condensed and returned to the reactor and (3) the product is continuously withdrawn and subjected to treatment af
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗