US 4,158,710 A#22706254 Most CitedExpiredUnited States (USPTO)Utility

Method of preparation of the surfaces of products made of iron alloys, preceding the process of hot-dip aluminizing

4Forward Citations (#22706254 Global)
0.1/yrCitation Velocity (#46510158 Global)
2.55Citation PageRank (#9828093 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The work-pieces are mechanically cleaned, degreased and washed, and then etched in an aqueous solution containing 0.5-1.0% by weight of citric acid, and 16-24% by weight of hydrochloric acid, having a temperature of 15°-30° C., preferably of 20°-25° C., for the time of 1-20 minutes, preferably 2-5 minutes, whereafter the work-pieces are neutralized in an aqueous ammonia solution having a concentration not exceeding 1% by weight, at a temperature of 15°-25° C., in a time not shorter than 1 minute. After being washed in water at a temperature not exceeding 35° C. in a time not shorter than 1 minute, they are dipped in an agitated aqueous solution of the flux, containing 1.8-2.5% by weight of potassium fluoride, 0.8-1.5% by weight of sodium fluoride, and 1.5-3.0% by weight of potassium fluorozirconate, having a temperature of 40°-80° C. After at least two minutes of holding in the flux, the work-pieces are dried and finally dipped in a melt of aluminum or alloys thereof. Alternatively a flux having composition 1.5-2.0% by weight of potassium fluoride, 1.5-2.0% by weight of sodium fluoride, 6.0-10.0% by weight of sodium tetraborate and 2.5-5.0% by weight of acetic acid, having a temper

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for treatment of a work-piece made of an iron alloy, said method comprising the steps of mechanically cleaning said work-piece, degreasing and washing the cleaned work-piece, etching the washed work-piece in an aqueous solution comprising 0.5-1.0% by weight of citric acid and 16-24% by weight of hydrochloric acid at a temperature of 15°-30° C. for 1-20 minutes, neutralizing the etched work-piece in an aqueous solution of ammonia having a concentration not exceeding 1% by weight at a temperature of 15°-25° C. for not less than 1 minute, washing the neutralized work-piece in water at a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗