Corrosion resistant refractory mix
Abstract
A corrosion resistant refractory mortar or castable mix is provided comprising a particulate mixture capable of mixture with water to form a castable refractory or mortar having enhanced corrosion resistance to molten aluminum which is particularly useful in the production of ultra high purity aluminum. The mixture consists essentially of 10 to 34 parts by weight calcium aluminate, 1.5 to 10 parts by weight of a zinc borosilicate frit and 60 to 88 parts by weight alumina. The zinc borosilicate frit consists essentially of 50 to 60% by weight zinc oxide, 20 to 40% by weight boron oxide, 8 to 12% by weight silicon oxide and 0 to 10% by weight aluminum oxide with less than 0.5% by weight of other impurities. The refractory mix contains not greater than 1% by weight impurities.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 9.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A particulate refractory mixture capable of mixture with water to form a refractory having enhanced corrosion resistance for usage in the production of ultra high purity aluminum consisting essentially of: 90 to 98.5% by weight refractory material and 1.5 to 10% by weight of a zinc borosilicate frit consisting essentially of 50 to 60% by weight zinc oxide, 20 to 40% by weight boron oxide, 8 to 12% by weight silicon oxide and 0 to 10% by weight aluminum oxide with less than 0.5% by weight impurities in the frit and not more than 1% by weight impurities in the refractory mixture.
- Claim 2Depends on #1
The mixture of claim 1 wherein said zinc borosilicate frit has a particle size of not greater than -100 mesh.
- Claim 3Depends on #1
The refractory mixture of claim 1 wherein said refractory material consists essential