Abstract
Compositions of and methods for the preparation of polyvinylpyridine and iodine (PVP.nI 2 ) as cathode materials for electrochemical cells.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 10.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of preparing a cathode material is improved conductivity comprising the steps of mixing a quantity of polymeric material selected from the group consisting of P2VP, P4VP and mixtures thereof with a quantity of iodine sealing the mixture in a sealed container and heating the mixture to a temperature of at least about 225° C. for a predetermined period of time.
- Claim 2Depends on #1
The method of claim 1 in which the heating temperature is between about 225° C. to about 320° C. and the heating time is about 1 hour.
- Claim 3Depends on #1
The method of claim 1 in which the polymeric material is P2VP.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (3)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,754,245 A | Interhalogen adducts of polyvinyl pyrrolidone | 1956 | 19 |
| US 3,136,755 A | Insoluble polymeric-iodine complexes | 1964 | 20 |
| US 4,027,083 A | Manufacture of polyvinylpyrrolidone-iodine | 1977 | 16 |