Room temperature cured elastomer

2Forward Citations (#34239213 Global)
0.0/yrCitation Velocity (#54995415 Global)
2.83Citation PageRank (#8343447 Global)
2Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Hydroxy terminated polybutadiene is reacted with naphtyl-potassium and 1-mo-2,4-pentadiene in successive steps to form a bis(1,3-pentadienyl ether) derivative. Then the bismaleimide of dimer diamine is added to the polybutadiene derivative whereby a room temperature cure to an elastomer is achieved.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing an elastomer which comprises the steps of: A. preparing the bis(1,3-pentadienyl ether) derivative of hydroxy terminated polybutadiene and B. curing said derivative with a bismaleimide of dimer diamine.