Method and apparatus for producing copper clad steel wire
Abstract
A method of producing a copper clad steel wire, which comprises the steps of preparing a 5 to 15 mm diameter steel rod and a 21 to 66.7 mm width copper tape; continuously supplying the steel rod and the copper tape separately and cleaning the surfaces thereof; forming the copper tape in tubular form such that the copper tape can cover the steel rod while supplying the steel rod and the copper tape in parallel, and welding the edges of the copper tape in a non-oxidizing atmosphere; sinking the tubular copper tape sufficiently for the copper tape to substantially come into contact with the steel rod to form a copper clad steel rod; cold-drawing the copper clad steel rod and/or hot working the clad rod at a temperature of 400° to 800° C. to reduce its cross-sectional area by more than 20%; and then annealing the copper clad steel rod at a temperature of 300° to 1050° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 30.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of producing a copper clad steel wire, comprising the steps of (a) preparing a 5 to 15 mm diameter steel rod and a 21 to 66.7 mm width copper tape, the steel rod and the copper tape having a relation expressed by ##EQU3## where r is the radius of the steel rod and t is the thickness of the copper tape; (b) continuously supplying and surface-cleaning the steel rod and the copper tape separately, forming the copper tape in tubular form such that the copper tape can cover the steel rod, and then welding the seam of the copper tape in a non-oxidizing atmosphere; (c) sinking the tubul
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗