In situ carbonate leaching and recovery of uranium from ore deposits
Abstract
Uranium ore deposits which contain certain proportions of other metals and elemental components, such as are present in redox roll front ore deposits, are selectively leached in situ by passing therethrough relatively dilute aqueous leach solutions comprising essentially from about 0.5 to 5 grams per liter of ammonium bicarbonate and from about 0.1 to 3 grams per liter of peroxide, preferably introduced as aqueous H2O2, and sufficient ammonia to bring the solution to a pH of from about 7.4 to 9, and preferably from 7.5 to 8.5, thereafter withdrawing from the ore deposit the aqueous leach solution enriched in uranium which it preferentially extracts along with a generally lower proportion of other metals and elements as compared to their respective ratios in the ore deposit, and contacting the enriched leach solution with a strong base anion exchange material to strip the uranium from the leach solution. The uranium is eluted by treating the base anion exchange material with an aqueous eluant, and finally the uranium is recovered from the uraniferous eluate by first acidifying it and then treating with ammonia to produce a precipitate of relatively pure ammonium diuranate. The strip
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 49.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
In the process of in situ leaching of uranium from ore deposits, the steps comprising: (a) passing through the ore deposit an aqueous leach solution of a pH of from about 7.4 to 9 comprising from about B 0.5 to 5 grams per liter of ammonium bicarbonate and from about 0.1 to 3 grams per liter of H 2 O 2 , the peroxide being added at a point to prevent substantial decomposition thereof before it comes into contact with the ore, (b) withdrawing from the ore deposit the enriched aqueous leach solution after it has been in contact with uranium of the ore deposit and dissolves uranium, and (c)
- Claim 2Depends on #1
The process of claim 1, wherein the peroxide is provided by an aqueous hydrogen peroxide soluton of at least 20% concentration of H 2 O 2 , wherein ammonia is added to
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 49 total)
References Cited — Backward Prior Art (10)
Non-Patent Literature (1)
- Proceedings of the Second United Nations International Conference on The Peaceful Uses of Atomic Energy, vol. 3, "Processing of Raw Materials", pp. 333-339 and 444 (1958), United Nations, Geneva.