Process for producing shock-proof graft copolymers of styrene with synthetic rubber

9Forward Citations (#11987168 Global)
0.2/yrCitation Velocity (#34609933 Global)
1.79Citation PageRank (#17291720 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The process for producing shock-proof graft copolymers of styrene with synthetic rubber consists in that rubber is dissolved in styrene at a maximum temperature of 75° C. The resultant solution is subjected to prepolymerization by being heated to 75-85° C. in the presence of a plasticizer and a peroxide initiating agent. The peroxide initiator is essentially a composition of the following formulation (in parts by weight): diacylated peroxides of aliphatic acids C 3 -C 5 , 2 to 8; diacylated peroxides of aliphatic acids C 6 -C 9 , 80 to 89; diacylated peroxides of aliphatic acids C 10 -C 12 , 7 to 14. The prepolymerization process proceeds until the 25-40 percent styrene conversion. The result is the prepolymer which is exposed to aqueous-suspension polymerization by being heated in an aqueous medium to maximum 140° C. at a prepolymer-to-water volume ratio ranging within 5:3 and 10:3, respectively, in the presence of peroxide polymerization; initiators and a stabilizing system, consisting of 0.15-1.5 wt. % tricalcium phosphate, 0.003-0.02 wt. % of a mixture of disubstituted sodium alkylsulphates of a general formula as such: R--OSO 3 Na, where R is a hydrocarbon radical, containing

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing shock-proof graft copolymers of styrene with synthetic rubber, residing in that rubber is dissolved in styrene at a maximum temperature of 75° C.; the resultant solution is subjected to prepolymerization by being heated to 75°-85° C. in the presence of a plasticizer and a peroxide initiating agent of the following formulation: diacylated peroxides of aliphatic acids C 3 -C 5 --2-8 weight parts; diacylated peroxides of aliphatic acids C 6 -C 9 --80-89 weight parts; diacylated peroxides of aliphatic acids C 10 -C 12 --7-14 weight parts, until 25-40 percent of th