Desulfurization of naphtha charged to bimetallic catalyst reforming
Abstract
A hydrocarbon fraction boiling below about 430° F. and initially desulfurized to contain not more than about 2 ppm weight of sulfur is further desulfurized to comprise less than 0.5 ppm sulfur by sequential contact with a desulfurizing catalyst and a bed of zinc oxide before effecting bimetallic reforming of a naphtha boiling fraction.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 28.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
In a combination process for upgrading a naphtha fraction by desulfurization to reduce sulfur in the naphtha charge to within the range of 0.5 to 5 ppm and the naphtha is thereafter reformed by contact with a bimetallic reforming catalyst at a temperature in the range of 870° to 1100° F., the method for improving the combination process which comprises, passing the naphtha product of desulfurization and comprising from 0.5 to 5 ppm of sulfur in admixture with recycle hydrogen gas in indirect heat exchange with the effluent product of the reforming operation in a sequence of heat exchange zones
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗