Methods for producing improved stable polyethylene terephthalate
Abstract
Methods for producing improved, thermally-stable polyethylene terephthalate resins are provided. Polyethylene terephthalate resins are provided that can be fabricated into products such as carbonated beverage containers with a minimum of degradation products such as acetaldehyde preferably by rapidly polymerizing a prepolymer from an i.v. of about 0.2 to an i.v. of at least about 0.7.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 36.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of producing an improved, stable, polyethylene terephthalate resin from a low-molecular weight prepolymer of ethylene glycol and terephthalic acid having an intrinsic viscosity of about 0.1 to 0.3, the method comprising the steps of: (A) Further polymerizing the prepolymer to a higher intrinsic viscosity of about 0.4 to 0.6 at a temperature of about 270° C. to 290° C. at a high reaction rate for less than about one-half hour; and (B) Further polymerizing the reaction product of Step (A) in a solid state to provide a stable resin with an intrinsic viscosity of at least about 0.7.
- Claim 2Depends on #1
A method as defined in claim 1 including the additional steps forming an article from the stable polyethylene terephthalate resin of Step (B).
- Claim 3Depends on #1
A method as defined in claim 1 and which the further polymerizing of Step (A) i