A method of denitriding a high chromium molten steel with a minimum chromium loss is disclosed. A high chromium molten steel containing 0.8-2.5% of C and 10-35% of Cr is denitrided to a final nitrogen content of not more than 40 ppm in a ladle under vacuum by flowing an inert gas into molten steel at a flow rate of not less than 15 Nl/min per ton of molten steel and at the same time blowing oxygen gas against molten steel until carbon content [C] in molten steel satisfies the following equations (1) and (2) in accordance with the carbon content prior to decarburization [C] of molten steel: [C]≦[C] 0.3, when 0.8≦[C]≦1.0% (1) [c]≦55/70[c]--6/70, when 1.0≦[C]≦2.5% (2).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 6.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of denitriding a high chromium molten steel to a nitrogen content of not more than 0.0040% with a minimum chromium loss using a vacuum ladle decarburization equipment, which comprises transferring a high chromium molten steel containing 0.8 to 2.5% of carbon, 10 to 35% of chromium and not more than 0.06% of nitrogen from a steel making furnace into a ladle, putting the ladle in a vacuum tank and then under a vacuum of not more than 60 Torr, flowing an inert gas into the molten steel at a flow rate of not less than 15 Nl/min per ton of molten steel from the bottom of the ladle and conc