Abstract

The invention relates to a method for the preparation of polyamides with enhanced electric conductivity (specific resistance below 10 9 Ω.cm) by the anionic polymerization of lactams with 7 to 13 atoms in the ring using the usual basic polymerization initiators and accelerating activators. The polymerization is carried out in the presence of 2-20 wt. parts of plasticizers, e.g. N,N-dialkoxy or N,N-dialkylacrylamides or methacrylamides or their polymers, polyethyleneoxide, polyamides or lactams of higher concentration of amide groups than has the principal lactam, and 1-50 wt. parts of a very finely ground graphite and/or conductive black per 100 wt. parts of anhydrous principal lactam or mixture of lactams.The polymerization is performed in a mold to give directly the required article or in continuous reactors to various profiles or to form granulates. The semiconductive polyamide, which is the product of this invention, is suitable, for instance, for use as machine parts operating under conditions where the formation of electrostatic charges should be eliminated (e.g. in mines, chemical plants, etc.) or for articles where the conductivity is usefully employed (e.g. low temperature

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 9.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Method for the preparation of semiconductive polyamides, having a specific electric resistance, measured at relative humidity of 50% and 25° C., of below 10 9 Ω.cm, by anionic polymerization comprising first forming a dispersed admixture of 100 weight parts of at least one anhydrous molten lactam containing 7-13 atoms in the ring, a basic polymerization initiator, an accelerating activator, 2-20 weight parts of at least one anhydrous hydrophilic plasticizer selected from the group consisting of N,N-dialkoxyacrylamide, N,N-dialkylmethacrylamide, N,N-dialkylacrylamide, N,N-dialkoxymethacrylamid

  2. Claim 2Depends on #1

    Method as set forth in claim 1, wherein said

Technical Overview & Description