Patents
US 4,152,482 A#6556304 Most CitedExpiredUnited States (USPTO)Utility

Anisotropic fibrous thermal insulator of relatively thick cross section and method for making same

14Forward Citations (#6556304 Global)
0.3/yrCitation Velocity (#25395609 Global)
7.41Citation PageRank (#1742338 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention is directed to an anisotropic thermal insulator formed of carbon-bonded organic or inorganic fibers and having a thickness or cross section greater than about 3 centimeters. Delaminations and deleterious internal stresses generated during binder curing and carbonizing operations employed in the fabrication of thick fibrous insulation of thicknesses greater than 3 centimeters are essentially obviated by the method of the present invention. A slurry of fibers, thermosetting resin binder and water is vacuum molded into the selected insulator configuration with the total thickness of the molded slurry being less than about 3 centimeters, the binder is thermoset to join the fibers together at their nexaes, and then the binder is carbonized to form the carbon bond. A second slurry of the fibers, binder and water is then applied over the carbonized body with the vacuum molding, binder thermosetting and carbonizing steps being repeated to form a layered insulator with the binder providing a carbon bond between the layers. The molding, thermosetting and carbonizing steps may be repeated with additional slurries until the thermal insulator is of the desired final thickn

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 14.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for fabricating a thermal insulating composite comprising an array of oriented fibers joined together by a carbonized binder and characterized by having anisotropic thermal properties and a wall thickness greater than about 3 centimeters, comprising the steps of: (a) forming a slurry of fibers of a carbonaceous or refractory material, a particulate thermosetting resin binder in a binder-to-fiber ratio of about 0.5 to 1.0, and water in a solids-to-water ratio of about 0.005 to 1.0 into a desired configuration by contacting a perforated mold of said configuration with a sufficient quant