Patents
US 4,152,408 A#1901805 Most CitedExpiredUnited States (USPTO)Utility

Fibrous calcium sulfate

33Forward Citations (#1901805 Global)
0.7/yrCitation Velocity (#10860095 Global)
9.77Citation PageRank (#1102666 Global)
5Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Fibrous calcium sulfate is produced by autoclaving a dilute aqueous suspension of gypsum, at a temperature between the minimum fiber forming temperature and about 20° C. above, in the presence of a dispersing agent to provide for discrete whisker crystal development and protecting the whisker crystals from destruction or conversion to a different physical or chemical form until they have been stabilized by calcining at a temperature in excess of 500° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 33.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of preparing a dispersible calcium sulfate fiber which comprises heating to a temperature above about 110° C. under autogenous pressure, an aqueous suspension comprising between about 5% and about 10% by weight of gypsum and between about 1 and 100 ppm based on the total weight of the gypsum suspension of tannic acid or a tannin as a dispersing agent, and thereafter recovering the fiber mass substantially free of three-dimensional entanglement by filtering and drying.

  2. Claim 2Depends on #1

    A process according to claim 1 wherein dispersing agent is tannic acid in an amount between about 5 and about 50 ppm based on the total weight of reaction mixture.

  3. Claim 3Depends on #1

    A process according to claim 1 wherein the dispersing agent is tannic acid in an amount between about 10 and about 30 ppm based on the total weight of reaction mixture.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗