Patents
US 4,152,142 A#1480830 Most CitedExpiredUnited States (USPTO)Utility

Recovery of copper values from iron-containing ore materials as mined and smelted

39Forward Citations (#1480830 Global)
0.8/yrCitation Velocity (#8675657 Global)
4.01Citation PageRank (#4750902 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for improving overall recovery of copper from an integrated mining and metallurgical processing operation by utilizing iron-containing copper ore materials as mined, such as low-grade copper ores and mine wastes, and crushed or granulated copper-containing slag obtained by smelting the higher-grade portions of such ore materials, involves the minign of such ore materials, the smelting of higher grade portions thereof, and the leaching of copper values from lower grade portions thereof with an aqueous, weakly acidic lixiviant to produce an acidic, ferric, effluent solution. The smelter slag is leached with the such effluent solution and copper values are recovered from the resulting pregnant solution. If desired, the barren solution may be recycled to the initial ore leaching step. By maintaining the pH of the acidic, ferric effluent solution from the initial leach within its normal range of about 1.9 to 3.0 for the slag leaching step, copper is selectively leached from the smelting slag while avoiding the usual precipitation of ferric salts and the formation of gelatinous slag decrepitation products. Moreover, ferric ion values in the acidic, ferric effluent solution from

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 39.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In the recovery of metallic copper from a copper-sulfide ore deposit containing pyrite, the steps of (a) mining the ore deposit; (b) smelting the higher grade ore mined from said deposit to yield a smelter slag containing relatively little copper; (c) leaching with an acidic ferric sulfate solution, of pH between about 2 and 3.5, rejected lower grade portions of the mined ore materials containing pyrite and relatively litte copper to yield a copper-bearing, acidic, ferric sulfate solution; (d) grinding or granulating said smelter slag; (e) leaching the ground or granulated smelter slag with th

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Flett "Solvent Extraction in Copper Hydrometallurgy : A Review" Inst. Min. & Met. Transactions" Sect. C, vol. 83, Mar. 1974, pp. C30, C31.
  • Shelley, "Methods for Recovering Copper from Waste Copper Smelting Slags by Leaching" Inst. Min & Met. Transactions Sect. C, Mar. 1975, pp. C1-C4.