Patents
US 4,151,336 A#1975803 Most CitedExpiredUnited States (USPTO)Utility

Process for the production of a substantially equimolecular copolymer of maleic acid anhydride and diisobutylene

33Forward Citations (#1975803 Global)
0.7/yrCitation Velocity (#10886143 Global)
3.20Citation PageRank (#6841697 Global)
2Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An improved process for the production of a substantially equimolecular copolymer of maleic acid anhydride and diisobutylene in which from 10 to 100 mole % of the anhydride groups are esterified with linear or branched aliphatic monoalcohols containing from 1 to 20 carbon atoms or with cycloaliphatic monoalcohols containing from 5 to 6 carbon atoms to form the corresponding semiesters, wherein shortly before or after the end of the solution or suspension copolymerization of maleic acid anhydride and diisobutylene a monomer corresponding to the general formula ##STR1## in which R=H, CH 3 , C 2 H 5 , --OR 2 , --O--CO--CH 3 , ##STR2## --CH 2 OH, --CH 2 O--C--CH 3 , R 1 =H , CH 3 and R 2 =a linear or branched alkyl group containing from 1 to 4 carbon atoms, Or mixtures of these monomers with one another are added to the polymerization mixture in quantities of from 1 to 12 mole %, based on the maleic acid anhydride used. The aqueous or aqueous-alcoholic alkali, amine or ammonium salt solutions of the semiesters of the copolymer are highly effective as anionic sizing agents for paper.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 33.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a substantially equimolecular copolymer of maleic acid anhydride and diisobutylene which comprises the steps of initiating solution or suspension copolymerization of maleic acid anhydride and diisobutylene and shortly before or after conclusion of said copolymerization introducing at least one additional monomer into the resulting polymerization mixture in an amount of from 1 to 12 mol %, based on the amount of maleic acid anhydride subjected to copolymerization, and maintaining resulting monomer containing polymerization mixture at a temperature of from 30° to 200° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗