Abstract

{PG,1 High melt flow olefin polymers suitable for such applications as injection molding, and the like requiring a narrow molecular weight distribution are produced using a catalyst made by reducing and reoxidizing a chromium catalyst on either a titanium-silica cogel or a self-reduced silica-containing composition. In the first embodiment, a cogel formed by coprecipitating silica and titania, and containing a chromium compound, is treated in a nonoxidizing atmosphere, such as CO, hydrogen, N{HD 2 {L or a material decomposable to these materials, and thereafter reoxidized. In the second embodiment, a titanium-free chromium containing catalyst is first heated in air or the like to dry the catalyst and oxidize the chromium after which it is heated in an inert atmosphere wherein the composition is self-reduced to give chromium in a lower valence state. The resulting self-reduced composition is then heated in a reducing ambient and then reoxidized as in the first embodiment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 128.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for activating a chromium-containing catalyst prepared by coprecipitating a titanium compound and silica to form a cogel comprising a first step wherein said catalyst is contacted with a nonoxidizing ambient at a temperature of at least 600° C. and a subsequent second step where it is contacted with an oxygen-containing oxidizing ambient at a temperature within the range of 450°-1000° C.

  2. Claim 2Depends on #1

    A method according to claim 1 wherein prior to said first step said catalyst composition containing at least a portion of said chromium in the form of CrO 3 is treated at a temperature of 600°-1100° C. in an inert atmosphere for a time sufficient to achieve at least partial self-reduction of said chromium to a lower valence state and wherein said nonoxidizing ambient of said first step is a reducing agent under the conditions employed in said f

Technical Overview & Description