Patents
US 4,151,058 A#796174 Most CitedExpiredUnited States (USPTO)Utility

Method for manufacturing a layer of amorphous silicon usable in an electronic device

54Forward Citations (#796174 Global)
1.1/yrCitation Velocity (#5394340 Global)
61.35Citation PageRank (#49935 Global)
3Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method aiming at imparting to the amorphous silicon properties which are compatible with the possibility of modifying by doping or field effect the position of the Fermi level in the volume of the amorphous silicon, a prime requirement for the operation of semiconductor devices. The method comprises a first step of depositing a layer of amorphous silicon onto a substrate under conditions ensuring the purity of the deposit obtained, then a second step wherein the deposit is subjected to a heat treatment consisting in maintaining the deposit in the atmosphere of a plasma containing atomic hydrogen for saturating the existing broken chemical bonds responsible for a parasitic electric conductivity.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 54.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a layer of high resistive amorphous silicon onto a substrate, said method comprising at least the following steps: (a) depositing under a partitial vacuum without adding hydrogen a layer of amorphous silicon onto said substrate; (b) maintaining said layer at a temperature between 100° C. and the temperature of crystallization of the amorphous silicon in an atmosphere of a plasma containing hydrogen or one of its isotopes to increase the resistivity of said amorphous silicon.

  2. Claim 2Depends on #1

    A method as claimed in claim 1, wherein, at step (a), amorphous silicon is deposited by cathodic sputtering on a substrate maintained at a temperature of more than 100° C.

  3. Claim 3Depends on #1

    A method as claimed in claim 1, wherein, at step (b), the plasma is created by an electric field of a frequency between 10 and 100 MHz i

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Comber et al., Electronic Transport and State Distribution in Amorphous SI Films, J. of Non-Crystalline Solids, 11/1972, pp. 219-234.
  • IBM Technical Disclosure Bulletin, vol. 19, No. 12, May 1977, Brodsky et al., Doping of Sputtered Amorphous Semiconductors.